What aluminium sheet is

Aluminium sheet is flat stock obtained by rolling from ingots. The requirements for it are set out in GOST 21631. The sheet in the catalog is from 0.5 to 10 mm thick, so it is used both as a thin cladding material and as a structural one. It is about three times lighter than steel sheet, does not rust and bends, stamps, drills and cuts well by mechanical and laser methods.

Which alloy to choose

TaskAlloys in the catalog
Cladding, roofing, decorAD0 (1050), AMts (3003)
Welded housings, bodies, tanksAMg2, AMg3, AMg5, AMg6
Shipbuilding and marine environmentAMg4.5 (5083)
Parts under loadD16 (2024), D1T, V95 (7075)
Structures strengthened by heat treatmentAD31 (6061 T6), AD35 (6082 T6)

What the letters and digits of the temper mean

M is the annealed soft temper, in which the sheet bends most easily. H is work-hardened by rolling: harder, stronger, but with limited bending. H111 denotes an almost annealed sheet, H22 and H24 a partially work-hardened one, and H321 a temper for 5000 series alloys that work in a marine environment. T3, T4 and T6 are strengthening by heat treatment, which raises strength but reduces plasticity. So H111 or M is taken for bending, and T for parts under load.

Formats and protective film

The width of the sheet in the catalog is 1000, 1250 or 1500 mm and the length is from 2000 to 4000 mm; common formats are 1000 by 2000 and 1250 by 2500 mm. The thicknesses are 0.5, 0.8, 1, 1.2, 1.5, 2, 2.5, 3, 4, 5, 6, 8 and 10 mm. There are items with a protective PVC film: it protects the surface during cutting, bending and installation and is removed after the work is finished.

Bending and welding

The bending radius depends on the alloy, temper and thickness: the harder the sheet, the larger the radius needed, otherwise the metal cracks. The bend line is best placed across the rolling direction. Aluminium is welded in argon. In alloys strengthened by heat treatment, for example 6061 and 6082, the strength next to the seam drops locally, so this fact is taken into account in the calculation of important units.

Common mistakes

  • taking a hard sheet for a small bend radius;
  • not stating the temper and giving only the alloy grade;
  • using a thin sheet without flanging where stiffness is needed.

Aluminium or steel sheet

Aluminium sheet is advantageous where low mass, corrosion resistance and ease of processing matter. But it is less stiff and less hard than steel, and it also expands more when heated. So when replacing steel with aluminium the thickness and shape of the part are recalculated, not copied. For cladding, housings and casings such a recalculation is usually enough, and the gain in weight is noticeable.

Surface and further finishing

The sheet is supplied with a factory surface. Before painting it is degreased and, if needed, primed with a special primer for aluminium, otherwise the paint holds badly. For visible parts it is convenient to take a sheet with a protective PVC film: it is removed only after installation, when the surface is no longer threatened by scratches. The sheet can also be anodized if a durable and decorative surface is needed.

How to choose and what to state

  • the thickness, width and length of the sheet;
  • the alloy and temper for the way of processing;
  • whether a protective film is needed;
  • the cutting plan if blanks are needed.