How aluminium differs from steel
Aluminium is about three times lighter than steel, does not rust thanks to a thin oxide film, conducts heat and current well and is easy to cut and bend. At the same time it is softer and less stiff: with the same cross-section an aluminium beam deflects more than a steel one. So a structure is not simply replaced one to one, but the section and wall thickness are recalculated.
Alloy groups
| Alloy | Features | Typical use |
|---|---|---|
| AD0, AD1 | Pure aluminium, soft and plastic | Strip, foil, cladding |
| AMts, AMg | Corrosion resistant, weld well | Tanks, bodies, ships, welded units |
| AD31 | Main profile alloy, anodizes well | Frames, structures, pipes, angles |
| D16, D1, V95 | High strength, weld poorly | Aircraft, loaded parts |
What the letters after the grade mean
The letter shows the temper of the material. M is annealed, soft and bends easily. H is work-hardened by rolling: harder and stronger, but bends worse. T is strengthened by heat treatment, the so-called duralumins. The digits after the letter specify the mode, for example T3, T4 or T6 for heat-treated alloys and H22 or H24 for work-hardened ones. In the catalog an international number in brackets often stands next to the grade, for example 6060 or 5083, which helps to match the item with foreign documents.
Range in the catalog
- sheets, plates, checkered sheets and strip;
- round, profile and oval pipes, including anodized ones;
- round, square and hexagon bars, flat bars and wire;
- profiles: angle, channel, T-section, I-beam, Z-section;
- aluminium powder and flake powder.
Cutting and welding
Aluminium cuts, bends, stamps and mills well. It is welded in argon by the TIG or MIG method with a filler wire, for example ER 4043 or ER 5356. Before welding the oxide film is removed from the edges, because it melts at a much higher temperature than the metal itself. High-strength alloys D16 and V95 weld poorly, so they are joined with rivets or bolts.
Common mistakes
- taking high-strength D16 instead of AMg or AD31 for a welded frame;
- not stating the temper (M, H or T), although bending depends on it;
- joining aluminium to steel without insulation at contact points where water is present.
Corrosion and contact with other materials
The oxide film protects aluminium in air, water and most neutral media, but it is destroyed by alkaline solutions: fresh cement mortar, concrete and strong detergents. So aluminium that is built into masonry or washed with aggressive chemicals is protected. To avoid galvanic corrosion, contact points with steel or copper in a damp environment are separated with gaskets, and fasteners are chosen compatible with aluminium.
Receiving and storage
On receiving, the grade and temper, size, length and the absence of dents and deep scratches are checked. The product is stored in a dry place on wooden supports, and sheets are interleaved with spacers. If aluminium lies for a long time in damp, white oxidation spots appear on it. They spoil the appearance, so such metal is better not left outdoors without a cover.
How to choose and what to state
- the type of product and the shape of the section;
- the size and length or the sheet format;
- the alloy and temper for the working conditions;
- the required cutting or surface treatment, for example anodizing.
Need a consultation?
Leave a request — we'll call you and help with selection and calculation.