What brass is

Brass is an alloy of copper with zinc to which lead, aluminium, tin or manganese are sometimes added. It is stronger than copper, well plastic, easy to machine and to work by pressure, resistant to corrosion and has a beautiful golden colour. Brass is non-magnetic and does not spark, so it is widely used in plumbing, fittings, electrical engineering, instrument making, musical instruments, hardware and decor.

Main grades

GradeFeaturesPurpose
L63Universal plastic brassStamping, bending, deep drawing
LS59-1Leaded, cuts well, fine chipsTurning, automatic machines
L68Plastic, with a higher copper contentDecor, radiators, drawing
L90 (tombac)Golden colour, very plasticDecor, jewellery and souvenir products
LAMш77-2-0,05Aluminium brass with arsenic, corrosion resistantHeat-exchange tubes

How to decode the grade

The letter L stands for brass, and the number after it is the copper content in percent, with the rest usually zinc. So L63 is about 63 percent copper. Additional letters point to alloying elements: S is lead, A is aluminium, Msh is arsenic. The numbers after the hyphen show their content. For example, LS59-1 has about 59 percent copper and one percent lead, and LAMsh77-2-0.05 has 77 percent copper, 2 percent aluminium and 0.05 percent arsenic. The composition is set by GOST 15527.

Range and standards

TypeStandardPurpose
Sheets and stripGOST 2208Stamping, radiators, hardware, decor
PipesGOST 494Heat exchangers, plumbing, instruments
Round and hexagon barsGOST 2060Valves, nuts, unions, turned parts
WireGOST 1066Fasteners, meshes, springs, brazing

Pressure working and cutting

Brass has its own grades for different kinds of processing. L63 suits cold working by pressure best: stamping, bending and deep drawing. LS59-1 with an addition of lead cuts well, gives fine chips and a clean surface, so it is chosen for turned parts on automatic machines. LS59-1 suits cold forming worse, and L63 gives longer chips in cutting, so each task takes its own grade.

Soldering and welding

Brass solders well with soft and hard solders with a suitable flux, so it is joined by soldering in plumbing, radiators and electrical engineering. It is harder to weld: zinc evaporates at high temperature, forming harmful fumes, and the seam turns out porous. So welding is done in a ventilated room, with protective equipment and with the modes for copper alloys, and where possible soldering is preferred.

Colour and tarnishing

The golden colour of brass depends on the copper content: the more of it, the more reddish the tone, as in tombac L90, and the more zinc, the yellower. In air and in a damp environment the surface gradually darkens. For decorative products it is polished and coated with a clear varnish or, on the contrary, artificially patinated. If a stable colour is needed, the way of protecting the surface is chosen before production starts.

Cracking and dezincification

Brass worked by cold deformation retains internal stresses. In an environment with ammonia vapours such products may with time become covered with cracks, which is called season cracking. To avoid it, after bending or stamping a low-temperature anneal is made to relieve the stresses. And in aggressive water zinc may leach out of the alloy, so for such conditions grades with inhibitors are chosen, for example with an addition of arsenic.

Lead and drinking water

Leaded brass LS59-1 contains about one percent of lead, which makes it excellent for machining. For products that come into contact with drinking water the requirements for lead content and the permitted grades depend on the norms, so they are clarified before ordering. For ordinary fittings, hardware, electrical engineering and parts of instruments leaded brass remains the main choice.

Receiving and storage

On receiving, the marking is checked against the brass grade, standard and batch, and the dimensions, the condition of the surface and the absence of deep scratches and stains are checked. Brass is stored in a dry room away from ammonia vapours, acids and moisture, because it darkens in air and in a damp environment. Sheets and strip are interleaved with paper, and different grades are kept separately, because they are easy to mix up by colour.

Common mistakes

  • taking LS59-1 for deep drawing or bending with a small radius;
  • not relieving stresses after cold forming in an ammonia environment;
  • welding brass without ventilation;
  • not stating the grade and condition and giving only the name "brass".

How to choose and what to state

  • the kind of product and the size;
  • the grade: L63, LS59-1, L68, L90 or another;
  • the standard and the condition as supplied;
  • the purpose: turning, stamping or soldering.

Related sections

Need a consultation?

Leave a request — we'll call you and help with selection and calculation.