What makes steel stainless

Stainless steel is an alloy of iron with chromium, of which there is at least 10.5 percent, and also with nickel, molybdenum, titanium and other elements. Chromium forms a thin invisible oxide film on the surface that protects the metal from corrosion and heals itself when damaged. Thanks to this, stainless products need no painting, keep their appearance for a long time and serve in water, damp air and food and chemical environments.

Main grades

GradeFeaturesWhere it is used
AISI 304Universal, welds and machines wellFood industry, equipment, architecture
AISI 316With molybdenum, more resistant in aggressive and salty environmentsChemistry, sea, chlorides
AISI 321Stabilised with titanium, works when heated and after weldingHeated and welded units
AISI 430Ferritic, magneticDecor, household appliances
AISI 310SHeat resistantFurnaces, heat exchangers
AISI 201With less nickel, inferior to 304 in corrosion resistanceDry interiors, decor

How to read the grade

In the catalog the grade is often written in several ways: by the AISI system, by the European standard EN and by GOST. For example, AISI 304 corresponds to EN 1.4301 and 08Kh18N10, AISI 321 to EN 1.4541 and 08Kh18N10T, AISI 316 to EN 1.4401. These are different names for one type of steel and not different materials, so such correspondences are convenient for comparing items and documents.

Range in the catalog

  • sheets and coils with different surface finishes;
  • seamless, welded round and profile pipes, matt and polished;
  • round, square and hexagon bars;
  • flat bars, angles and wire, including those of heat-resistant alloys.

Corrosion and chlorides

In ordinary conditions and in contact with food, AISI 304 is enough. In an environment with chlorides, for example near the sea, in swimming pools or when chlorine detergents are used, pitting may appear on the surface of 304. For such conditions AISI 316, which contains molybdenum, is taken. If resistance when heated or after welding is needed, AISI 321 stabilised with titanium is chosen.

Magnetism

A magnet does not show whether the steel is good or not. Austenitic grades 304, 316 and 321 are practically non-magnetic in the annealed state, but after cold deformation, welding or bending they may become slightly magnetic. Ferritic AISI 430 is always magnetic. So a check with a magnet only lets one tell ferritic steel from austenitic, and the exact grade is confirmed by the batch documents.

Machining and welding

Stainless steel is stronger and conducts heat worse than carbon steel and work-hardens strongly during deformation. So it is cut with a sharp tool, with a constant feed and cooling, and in bending the stronger springback is taken into account. It is welded in argon. For welded structures in corrosive environments grades with stabilisation or low-carbon ones are taken, and after welding the seam is cleaned and passivated.

Iron on the surface and rust stains

Stainless steel does not rust by itself, but particles of ordinary steel that land on its surface quickly become covered with rust and spoil the appearance. They remain from grinding wheels, brushes, cutting tools and from contact with steel racks. So separate tools and brushes are used for stainless steel, and after cutting and welding the surface is cleaned, pickled and passivated to restore the protective film.

Receiving and storage

On receiving, the marking is checked against the steel grade, standard and batch, and the dimensions, the condition of the surface, the presence of a protective film and the absence of rust stains are checked. The product is stored in a dry covered place, on wooden or plastic supports and separately from carbon steel so that there is no contact. The protective film is removed only after installation, and scratches on the surface are avoided from the first day.

Common mistakes

  • taking 304 for an environment with chlorides where 316 is needed;
  • considering a magnet proof of the grade;
  • working with steel brushes and wheels that leave iron;
  • not stating the standard or the surface and getting a different product.

How to choose and what to state

  • the environment and the working temperature;
  • the shape, size and length or format;
  • the grade and the standard: AISI, EN or GOST;
  • the surface finish and the needed cutting.

Related sections

Need a consultation?

Leave a request — we'll call you and help with selection and calculation.