What tempering is

Tempering is heating hardened steel to a certain temperature below the critical one with holding and subsequent cooling. After hardening steel is very hard but brittle and has large internal stresses. Tempering reduces brittleness and stresses and gives the needed combination of hardness and toughness depending on the tempering temperature.

Three kinds of tempering

TypeTemperatureWhat it givesPurpose
LowAbout 150–250 °CKeeps high hardness, reduces stressesCutting tools and measuring parts
MediumAbout 350–500 °CRaises elasticitySprings, leaf springs and dies
HighAbout 500–650 °CThe best balance of strength and toughnessImportant machine parts

The balance of hardness and toughness

The higher the tempering temperature, the softer and tougher the steel but the less hard. Lower tempering leaves almost all the hardness, so it suits a tool that must cut. High tempering noticeably reduces hardness but the part withstands blows and alternating loads. So the temperature is chosen not at random but for the purpose of the part and it depends on the grade of steel and the needed hardness.

When tempering is done

Tempering is done after hardening without delay, because a hardened part with large stresses may be damaged even before tempering. It is typically used for tools and tooling, shafts, axles, gears, springs and parts that work under impact load. For carburised parts tempering is also mandatory: after hardening of the surface it relieves stresses and makes the layer less brittle.

Duration of the treatment

Besides temperature, holding and cooling matter. The part must heat evenly across the whole section, so large and thick parts are held longer than thin ones. The duration together with the temperature is picked for the grade of steel and the requirements for hardness. After tempering the part is usually cooled in air and for some steels repeated tempering is applied.

What is tempered

  • cutting tools and measuring parts;
  • springs, leaf springs and dies;
  • shafts, axles, gears and pins;
  • tooling and parts under impact load.

What to state in an order

  • the grade of steel or metal of the parts;
  • the dimensions, shape and quantity of the parts;
  • the needed hardness after tempering;
  • a drawing if there are requirements for hardness on separate areas.

Temper brittleness

For some alloy steels there are ranges of tempering temperatures at which toughness, on the contrary, falls. This phenomenon is called temper brittleness. To avoid it, the mode and the cooling rate after tempering are picked for the particular grade and the temperature from the dangerous range is avoided. So the grade of steel is always stated and not only the needed hardness.

Hardness control

After tempering hardness is checked with a special instrument: this shows whether the part has fallen into the needed range. If the hardness turned out higher than needed, tempering can be repeated at a higher temperature, but a part that is softened too much will have to be hardened again. So when the range of hardness is strict, it is better to state it in the order rather than rely on a typical mode.

Common mistakes

  • putting off tempering after hardening;
  • not stating the needed hardness and getting a part that is too soft or too hard;
  • choosing high tempering for a tool that must cut.