Metal tempering
Tempering is done after hardening: it reduces brittleness and internal stresses and gives the required balance of hardness and toughness. We temper steel parts and tools to your order.
More about the serviceWhat we do
- Tempering after hardening
- Reducing brittleness and internal stresses
- Selecting the balance of hardness and toughness of the part
- Tempering tools and equipment
- Advice on choosing the heat treatment
Advantages
- Less brittlenessReduces brittleness after hardening
- Fewer stressesRelieves internal stresses
- Balance of propertiesThe required combination of hardness and toughness
- Mode to suit the steel gradeTemperature and duration are chosen to suit the grade and hardness requirements
Metals we work with
How it works
- 1Send the detailsSteel grade, dimensions, number of parts and required hardness
- 2QuoteWe choose the mode and calculate cost and terms
- 3TemperingWe temper the hardened parts using the chosen mode
- 4DeliveryWe hand over the parts or deliver across Ukraine
What we need for an order
- Steel grade
- Part dimensions
- Number of parts
- Required hardness
- Desired deadline
What the cost depends on
- Steel grade, size and number of parts
- Type of tempering: low, medium or high
- Required hardness
- Duration of the treatment
We name the exact cost after clarifying the details.
Need a quote?
Leave a request — we'll contact you, clarify the details and give you a price.
Frequently asked questions
What types of tempering are there?
Low (approximately 150–250 °C) — keeps high hardness and reduces stresses; for cutting tools and measuring parts.
Medium (approximately 350–500 °C) — increases elasticity; for springs, leaf springs and dies.
High (approximately 500–650 °C) — the best balance of strength and toughness; for critical machine parts.
When is tempering done?
After hardening: for tools and tooling, shafts, axles, gears, springs and parts that work under impact loads.
What does the tempering temperature depend on?
The duration and temperature are chosen to suit the steel grade and hardness requirements.
Is delivery available?
Yes, we deliver orders across Ukraine.
Useful articles
All articles →Often ordered together
Tempering: less brittleness and the right balance of properties
Tempering is heating hardened steel to a certain temperature (below the critical one) with holding and subsequent cooling. After hardening the steel is very hard but brittle and has large internal stresses. Tempering reduces brittleness and stresses and gives the required combination of hardness and toughness depending on the tempering temperature.
Types of tempering
- low (about 150–250 °C) — keeps high hardness, reduces stresses; for cutting tools and measuring parts;
- medium (about 350–500 °C) — increases elasticity; for springs, leaf springs and dies;
- high (about 500–650 °C) — gives the best balance of strength and toughness; for critical machine parts.
Where it is used
Tempering is performed after hardening for tools and tooling, shafts, axles, gears, springs and parts working under impact loads. The duration and temperature are chosen for the steel grade and the hardness requirements.
Ready to place an order?
Tell us what you need: grade, size and quantity — we will call you and find a solution.
Our advantages
Certified metal
The grade and standard (GOST, DSTU, EN) are given for every item in the catalog.
Warehouses and production
Warehouses in Kyiv, Kharkiv, Dnipro and Lviv; cutting and machining to your sizes.
A team of specialists
We will help you choose the grade, size and processing.
Individual approach
We will adapt cutting, volume and delivery across Ukraine to your task.